PDMS layers for microscopy sample chambers were spin-coated while studying how bacterial motility affects attachment to oil droplets.
PDMS layers for microscopy sample chambers were spin-coated while studying how bacterial motility affects attachment to oil droplets.
Reported: 100 mm silicon wafer, 100 rpm for 30 s, 1–1.5 mm PDMS layer.
University of Houston — Narendra K. Dewangan and Jacinta C. Conrad. 2020. Bacterial motility enhances adhesion to oil droplets. DOI: 10.1039/D0SM00944J.
Equipment reference: PDF p. 2; §2.6 Sample chamber preparation.
No Brewer Science authorship identified in source.