Siloxane cladding and core layers were spin-coated on silicon to evaluate optical losses during waveguide curing and aging.
Siloxane cladding and core layers were spin-coated on silicon to evaluate optical losses during waveguide curing and aging.
The source reports 800 rpm for a 50 µm cladding layer. Other curing equipment is separately described.
Georgia Institute of Technology — Shashikant G. Hegde. 2008. Investigation of Optical Loss Changes in Siloxane Polymer Waveguides During Thermal Curing and Aging.
Equipment reference: PDF p. 65; experimental fabrication.
No Brewer Science authorship identified in source.
Open original source ↗Application summary prepared by Cee. The original source remains the authority for its methods and findings.