Copper-powder dispersions were spin-coated on silicon to produce particulate electrodes for high-density capacitor arrays.
Copper-powder dispersions were spin-coated on silicon to produce particulate electrodes for high-density capacitor arrays.
Reported: 400 rpm for 40–60 s, yielding 5–10 µm particulate films. Distinct from the earlier copper-foil barium-titanate capacitor work.
Georgia Institute of Technology — Kanika Sethi. 2010. High-Density Capacitor Array Fabrication on Silicon Substrates.
Equipment reference: PDF p. 72; printed p. 57.
No Brewer Science authorship identified in source.