Thesis
Novel crystallization platforms for drugs and biomolecules: self-assembled surface functionalization and gelsApogee spin coater
The study reports SU-8 coating and bake stages for nanoindentation.
The method identifies a Cee® 200CBX for SU-8 application and a Cee® 1300X for baking. Nanoindentation is used to compare the coated wafers at different bake stages.
The process details describe the cited work. Reported recipes and results depend on the authors’ materials, substrates, and equipment configuration. Materials recorded for this reference include SU-8.
PubMed Central. Nanoindentation Analysis of SU-8 Coated Wafers at Different Baking Phases.
Open original source ↗Application summary prepared by Cee. The original source remains the authority for its methods and findings.