Paper / report

Cee® 1300CSX thermal-slide comparison of wafer-bonding adhesives

This industry study combines Corning glass-carrier expertise with Brewer Science materials research. It is Brewer-coauthored work.

How Cee® equipment is used

The Experimental section names a Cee® 1300CSX thermal-slide debonder. Figures 4–5 report release-force and velocity comparisons.

Equipment reported
Cee® 1300CSX
Source type
Conference research paper
Publication year
2015
Materials
BrewerBond, Temporary Bonding Adhesive
Substrate
Not reported
Source
Corning and Brewer Science, CS MANTECH

Process context

The reported comparison used Crystalbond wax at 85 °C and BrewerBOND 220 at 190 °C. Debond-test wafer diameter is not specified.

Source and equipment evidence

Hladik M, Shorey A. 2015. Improvements in Processing – Carrier and Material Impacts. CS MANTECH, May 18–21, pp. 81–84.

Equipment reference: Experimental, p. 81; thermal-slide results and Figures 4–5, p. 83.

Open original source ↗

Application summary prepared by Cee. The original source remains the authority for its methods and findings.

SEMICON EUROPA · 10–13 NOVEMBER

Bring your process questions.

Meet Jacob, CEE’s Global Sales Director, in Munich with our partner SiSTEM Technology.

Stand C1353 · Messe München
Spin coating, bake and chill, temporary bonding and debonding.

Book a stand meeting →

Mention Jacob from CEE in SiSTEM’s booking form.